الکترود قلیایی AMA 1184F
موارد مصرف:
DIN Standard: St 37-2 to St 60-2; St 37-3 to St 52-3; St 37.0 to ST 52.0; St 37.4 to St 52.4; StE 210.7 to StE 360,7; StE 210.7 TM toStE 360.7 TM; St 35.8 to St 45.8; HI; HII; 17mn 4 GL-A 36 to GL-E 36; StE 255 to StE 355; WStE 255 to WStE 355; TStE 255 to TStE 355; TT ST 35 N; GS-38; GS-52
EN Standard: S235JR to E335; S235J2G3 to S355J2G3; P235T1 to P355T1; P235T2; P355T2; L210 to L360NB; L290MB to L360MB; P235G1TH; P255G1TH; P235GH; P265GH; P295GH; S355G1S to S355G3S; S255N to S355N; P255NH to P355NH; S255NL to S355NL.
ASTM Standard: A27 a.A36 Gr.all; A214; A242 Gr. 1-5; A266 Gr. 1, 2, 4; A283 Gr. A, B, C, D; A285 Gr.A, B, C; A299 Gr.A, B; A328; A366; A515 Gr.60, 65, 70; A516 Gr.55; A570 Gr.30, 33, 36, 40, 45; A572 Gr.42, 50; A606 Gr.all; A607 Gr.45; A656 Gr.50, 60; A668 Gr.A, B; A907 Gr.30, 33, 36, 40; A841; A851 Gr.1, 2; A935 Gr.45; A936 Gr.50. APl 5 L Gr. B, X42-X56
ملاحظات:
- فقط الکترود خشک مصرف شود.
- خشک کردن مجدد : به مدت 2 ساعت در دمای 300 تا 350 درجه سانتیگراد.
- توضیحات
- توضیحات تکمیلی
- نظرات (0)
توضیحات
Standards: AWS/ASME SFA – 5.1 : E 7016–1–H8
DIN 8529 : E Y 42 67 Mn B H5
EN 499 : E 42 6 B 42 H5
خواص و کاربرد:
الکترود قلیایی کم هیدروژن که جوشی عاری از ترک با چقرمگی بالا در هر دو حالت بدون عملیات حرارتی و تنشزدایی شده ایجاد میکند. به دلیل بالا بودن خواص متالوژیکی فلز جوش، چقرمگی CTOD در دمای 10- درجه سانتیگراد عالی میباشد. این الکترود برای جوشکاری پاس ریشه مناسب بوده و دارای قوس پایدار و متمرکزی میباشد.
توضیحات تکمیلی
برند | آما |
---|
نقد و بررسیها
هنوز بررسیای ثبت نشده است.